In April 2016 Manchester eScholar was replaced by the University of Manchester’s new Research Information Management System, Pure. In the autumn the University’s research outputs will be available to search and browse via a new Research Portal. Until then the University’s full publication record can be accessed via a temporary portal and the old eScholar content is available to search and browse via this archive.

Investigation into non-aqueous remedial conservation treatments for iron-tannate dyed organic materials

Wilson, Helen Louise

[Thesis]. Manchester, UK: The University of Manchester; 2013.

Access to files

Abstract

Iron-tannate dyes have been used for thousands of years and on many continents to colour materials that are now part of our cultural heritage shades of black, grey, or brown. Cellulosic and proteinaceous yarns and woven textiles have been dyed with iron-tannate dyes to form objects or components of objects for domestic and ceremonial use. Unfortunately, the longevity and useful lifetime of iron-tannate dyed objects is threatened by the dye itself which accelerates the degradation of organic materials through metal-catalysed oxidation and acid-catalysed hydrolysis. The accelerated degradation causes weakening, discolouration, and embrittlement of the organic materials at a faster rate than undyed equivalents and if left unimpeded, weakens the objects to the point that they are no longer able to be exhibited without damage. In some cases the degradation is so great that the dyed areas of the objects have crumbled to dust. At present there is no suitable chemical stabilisation method available with which to inhibit this degradation. An aqueous treatment is available for successfully stabilising paper containing iron gall ink; iron gall ink is chemically similar to iron-tannate dye. However, the aqueous nature of this treatment makes it unsuitable for weakened fibres, water soluble components, and water sensitive materials which may be part of a composite material containing iron-tannate dye. Non-aqueous treatments are therefore urgently needed in order to preserve our iron-tannate dyed cultural heritage for future generations.In this project a range of non-aqueous antioxidants and a non-aqueous deacidifier (described in Chapter 8) were tested alongside existing aqueous treatment in order to establish their ability to slow down the degradation of a range of model iron-tannate dyed textiles (Chapters 9 and 10). Model textiles were developed as part of the project (Chapters 3-5) to be substitutes for historic materials in these stabilisation studies. Validation of the model textiles for this purpose (Chapter 6) involved the comparison of the model textiles with selected historic iron-tannate dyed objects within the British Museum’s collection (Chapter 6). The historic objects and the properties of the model textiles before and after accelerated ageing (Chapters 5 and 6) and before and after treatment application (Chapters 9 and 10) have been characterised using a variety of analytical techniques (Chapter 2). In order to determine which accelerated ageing conditions were the most suitable for this project various combinations of elevated temperature and either cycling or stable relative humidity were tested for their ability to produce noticeable changes in the properties of the dyed model textiles within four weeks of ageing (Chapter 7). This project is an AHRC/EPSRC funded Science and Heritage Programme PhD in which the British Museum has been a collaborative institution. Among other wider dissemination methods, research from this project has been presented to the public on numerous occasions at gallery tours and Science Day events at the British Museum.

Additional content not available electronically

5 x 5 cm pieces of the model textiles produced in this PhD project will be included in the printed copies of the thesis in Appendix 7.

Bibliographic metadata

Type of resource:
Content type:
Form of thesis:
Type of submission:
Degree type:
Doctor of Philosophy
Degree programme:
PhD Materials
Publication date:
Location:
Manchester, UK
Total pages:
513
Abstract:
Iron-tannate dyes have been used for thousands of years and on many continents to colour materials that are now part of our cultural heritage shades of black, grey, or brown. Cellulosic and proteinaceous yarns and woven textiles have been dyed with iron-tannate dyes to form objects or components of objects for domestic and ceremonial use. Unfortunately, the longevity and useful lifetime of iron-tannate dyed objects is threatened by the dye itself which accelerates the degradation of organic materials through metal-catalysed oxidation and acid-catalysed hydrolysis. The accelerated degradation causes weakening, discolouration, and embrittlement of the organic materials at a faster rate than undyed equivalents and if left unimpeded, weakens the objects to the point that they are no longer able to be exhibited without damage. In some cases the degradation is so great that the dyed areas of the objects have crumbled to dust. At present there is no suitable chemical stabilisation method available with which to inhibit this degradation. An aqueous treatment is available for successfully stabilising paper containing iron gall ink; iron gall ink is chemically similar to iron-tannate dye. However, the aqueous nature of this treatment makes it unsuitable for weakened fibres, water soluble components, and water sensitive materials which may be part of a composite material containing iron-tannate dye. Non-aqueous treatments are therefore urgently needed in order to preserve our iron-tannate dyed cultural heritage for future generations.In this project a range of non-aqueous antioxidants and a non-aqueous deacidifier (described in Chapter 8) were tested alongside existing aqueous treatment in order to establish their ability to slow down the degradation of a range of model iron-tannate dyed textiles (Chapters 9 and 10). Model textiles were developed as part of the project (Chapters 3-5) to be substitutes for historic materials in these stabilisation studies. Validation of the model textiles for this purpose (Chapter 6) involved the comparison of the model textiles with selected historic iron-tannate dyed objects within the British Museum’s collection (Chapter 6). The historic objects and the properties of the model textiles before and after accelerated ageing (Chapters 5 and 6) and before and after treatment application (Chapters 9 and 10) have been characterised using a variety of analytical techniques (Chapter 2). In order to determine which accelerated ageing conditions were the most suitable for this project various combinations of elevated temperature and either cycling or stable relative humidity were tested for their ability to produce noticeable changes in the properties of the dyed model textiles within four weeks of ageing (Chapter 7). This project is an AHRC/EPSRC funded Science and Heritage Programme PhD in which the British Museum has been a collaborative institution. Among other wider dissemination methods, research from this project has been presented to the public on numerous occasions at gallery tours and Science Day events at the British Museum.
Non-digital content not deposited electronically:
5 x 5 cm pieces of the model textiles produced in this PhD project will be included in the printed copies of the thesis in Appendix 7.
Thesis main supervisor(s):
Thesis co-supervisor(s):
Language:
en

Institutional metadata

University researcher(s):

Record metadata

Manchester eScholar ID:
uk-ac-man-scw:191168
Created by:
Wilson, Helen
Created:
1st April, 2013, 11:23:36
Last modified by:
Wilson, Helen
Last modified:
10th April, 2013, 11:15:30

Can we help?

The library chat service will be available from 11am-3pm Monday to Friday (excluding Bank Holidays). You can also email your enquiry to us.